F593 Alloy Group 7

Alloy Group 7

Precipitation Hardening Alloys

Condition Marking Diameter Range  Tensile, ksi Yield, ksi min Rockwell Hardness 
AH F593U ¼ to 1-1/2 135 to 170 135 C28 to 38 